Originally Posted By: Patrick0525
I am surprised by the high moly count.
But what concerns me is amount of Fe, Si, Na, K and Al. It is a high baseline ppm that will throw off my next UOA.
Moly, & boron, are pretty high in this. Looks like someone put Ceratec in a M1 or something, LOL.
Silicon is very normal, even kind of low here, as Si shows up in Anti-Foam additives.
The high-ish Fe might come from pipes, maybe the Al too. Those are wierd to see even that high, but not a problem.