First UOA on my S2000, changed early due to hard driving including one track day. Car has approximately 150,000km on the clock (90,000 miles) with 1000 miles on this oil.
Short OCI conducted as I was eager to check up on the motor following valve retainer replacement and following the vehicle's first track day.
Penrite Racing 10w40 was used, no doubt would've been safe to go much further and I will do so on the next batch of oil.
Can I get thoughts on the wear metals in the images below? I'm worried Iron, Aluminium and Lead are high on such a short interval.
Thank you!
Short OCI conducted as I was eager to check up on the motor following valve retainer replacement and following the vehicle's first track day.
Penrite Racing 10w40 was used, no doubt would've been safe to go much further and I will do so on the next batch of oil.
Can I get thoughts on the wear metals in the images below? I'm worried Iron, Aluminium and Lead are high on such a short interval.
Thank you!
Last edited by a moderator: