Mistubishi Magna 2002 (Diamante) 4sp auto @ 202,000km (125k miles).
Runs though an external cooler after the radiator then back through a magnefine filter.
Alum 11
Copper 14
Chrom Iron 35
Lead 2
Tin Magnes 1
Moly Boron 89
Sodium 1
Potas Calcium 82
Zinc 8
Phosph 203
Silicon 6
FTIR
Oxidation 31
Nitration 4
Water
PHYSICAL
Visc @40°C 28
PQ Index 24
Not sure if I should change it just yet. It looks ok on the dipstick but appeared dark in the bottle. I think the cooler and filter are doing a good job.
Runs though an external cooler after the radiator then back through a magnefine filter.
Alum 11
Copper 14
Chrom Iron 35
Lead 2
Tin Magnes 1
Moly Boron 89
Sodium 1
Potas Calcium 82
Zinc 8
Phosph 203
Silicon 6
FTIR
Oxidation 31
Nitration 4
Water
PHYSICAL
Visc @40°C 28
PQ Index 24
Not sure if I should change it just yet. It looks ok on the dipstick but appeared dark in the bottle. I think the cooler and filter are doing a good job.
Last edited: