Here is the UOA for Honda 5 speed automatic. The car is Crv 2014 with 86k mi. I did a 3x drain n refill 8.6k mi ago with (2/3) Amsoil SS ATL and (1/3) DW1 and added HSS shift restore later (at 1 oz/qt). Comparing to other Honda ATF UOA I think the wear metals are OK, but since the milage on the oil is still low some might have not be accumulated enough to be detected.
The oxidation is mostly indicator of esters AFIK since the oil still "looks" fresh and I forgot to mention signature series...
The analyzer didn't read the memo about DW1, so is wondering where zinc/magnezium are coming from (it's DW1, VOA)
The oxidation is mostly indicator of esters AFIK since the oil still "looks" fresh and I forgot to mention signature series...
The analyzer didn't read the memo about DW1, so is wondering where zinc/magnezium are coming from (it's DW1, VOA)